With the development of society and the continuous improvement of consumer demands for products, the demand and requirements for circuit boards will continue to increase. Nowadays, rigid-flex board factories of all sizes are developing rapidly. At the same time as they develop, quality problems and technical problems in the production of rigid-flex boards are also constantly emerging. Common quality problems with rigid-flex boards include the following:

1. Poor soldering


This is due to the contamination of the board surface during the production process of the Solution: Ensure that the hard-soft board manufacturer avoids contamination of the pad surface during the production process, ensures the humidity of the hard-soft board during long-term storage, and avoids moisture storage, especially gold boards, because gold boards are more susceptible to oxidation.soft-hard composite board or the contamination of the board surface during later storage.


2. The hole copper thickness is not enough and the hole copper plating is uneven.


This is a problem in the immersed copper plating process. For a PCB with a normal IPC standard 35um surface copper thickness, the hole copper thickness should range from 18-25um. However, in general small-scale circuit board PCB factories, the production operations are not standardized, and the testing methods do not have strict requirements. The quality of the purchased raw materials (copper balls) may not be up to standard, so that the thickness of the copper holes in the finished circuit board PCB is far less than the standard (the thickness of the hole copper is 10-15um, which is far less than the industry standard). However, this problem cannot be discovered during the electrical testing process. The result is that the hard-soft board is a good one in the hands of the customer. However, after reprocessing (SMT, wave soldering, post-soldering, power-on test, etc.), the hard-soft board will have an open short circuit. If the hard-soft board is broken, the hole copper will be broken.


This problem is difficult to find in the hands of customers. Problems such as open and short circuits can only occur after the parts are welded and powered on for testing. Characteristics of the defect pattern: The copper thickness of the hole is thin and the distribution between the hole opening and the middle of the hole is relatively uniform, and there is no obvious difference with the copper after the soldering mask is removed. There will be no phenomenon that the pattern is concentrated at the hole opening and is too thin. This is due to insufficient deposition of the electroplating itself and there is no erosion phenomenon.

Rigid-soft board untitled-1


Shenzhen CZY Circuit Co., Ltd. is a high-tech enterprise specializing in the R & D, manufacturing and sales of PCB circuit boards and metal-based circuit boards.

QUICK LINK

CATEGORY

CONTACT US
Andy Chen: +86 - 17820397306
Mr. Lin: +86 - 13632666620
Email: sales@czypcb.com
Copyright Shenzhen CZY Circuit Co.,Ltd.  All rights reserved.